Aug 10, 2017 Grinding–Magnetic Separation Processing for Upgrading Titanium Slag. Low-intensity magnetic separation was conducted to remove the iron particles embedded in the melting slag. The fineness of these particles was improved by decreasing the size of 80% of the particles to below 45 μm, after which a magnetic field intensity of 75 mT was applied. Through magnetic separation process